Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of BERGAMID® A700MOS2 - PA66 - Avient Corporation

Material Data Center offers the following functions for BERGAMID® A700MOS2:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Bergamid A datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Product Texts
Resistant. Negligible, reversible or no changes in mass and dimensions.

Please consider the information about the application of the materials.
Mechanical propertiesdry / condUnitTest Standard
ISO Data
Tensile Modulus 1600 / 3200 MPa ISO 527
Yield stress 60 / 80 MPa ISO 527
Yield strain 25 / 4 % ISO 527
Nominal strain at break >50 / 20 % ISO 527
Charpy impact strength, +23°C N / N kJ/m² ISO 179/1eU
Charpy impact strength, -30°C N / N kJ/m² ISO 179/1eU
Charpy notched impact strength, +23°C 25 / 6 kJ/m² ISO 179/1eA
Charpy notched impact strength, -30°C - / 4 kJ/m² ISO 179/1eA
Thermal propertiesdry / condUnitTest Standard
ISO Data
Melting temperature, 10°C/min 261 / * °C ISO 11357-1/-3
Temp. of deflection under load, 1.80 MPa 80 / * °C ISO 75-1/-2
Temp. of deflection under load, 0.45 MPa 220 / * °C ISO 75-1/-2
Coeff. of linear therm. expansion, parallel 85 / * E-6/K ISO 11359-1/-2
Coeff. of linear therm. expansion, normal 82 / * E-6/K ISO 11359-1/-2
Burning behav. at 1.5 mm nom. thickn. V-2 / * class IEC 60695-11-10
Thickness tested 1.5 / * mm -
Yellow Card available yes / * - -
Electrical propertiesdry / condUnitTest Standard
ISO Data
Relative permittivity, 1MHz 5 / 3.6 - IEC 62631-2-1
Dissipation factor, 1MHz 2000 / 300 E-4 IEC 62631-2-1
Volume resistivity 1E10 / 1E13 Ohm*m IEC 62631-3-1
Surface resistivity * / 1E10 Ohm IEC 62631-3-2
Electric strength 80 / 120 kV/mm IEC 60243-1
Comparative tracking index 600 / - - IEC 60112
Other propertiesdry / condUnitTest Standard
Water absorption 8.5 / * % Sim. to ISO 62
Humidity absorption 2.8 / * % Sim. to ISO 62
Density - / 1140 kg/m³ ISO 1183
Material specific propertiesdry / condUnitTest Standard
ISO Data
Viscosity number 150 / * cm³/g ISO 307, 1157, 1628
Test specimen productionValueUnitTest Standard
ISO Data
Injection Molding, melt temperature 280 °C ISO 294
Injection Molding, mold temperature 40 °C ISO 294
Characteristics
Processing
Injection Molding
Delivery form
Pellets
Regional Availability
Europe
Other text information
Injection Molding
Resistant. Negligible, reversible or no changes in mass and dimensions.

Please consider the information about the application of the materials.
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.